Which technique reaches which bonds?

all tools

Wavenumber coverage of the vibrational techniques in this class, against where the bonds of interest absorb. The metal–adsorbate bonds sit where infrared on supported catalysts goes blind.

Solid bar: routine. Pale bar: possible but limited (support absorption, detector or window cut-off, elastic peak). Ranges are typical working values and depend on detector, windows, laser and sample. The O-PTIR bar is the laser range of the CFN mIRage.
Raman: inelastic light scattering, needs a polarizability change, so it complements IR. Strong for oxide lattices, M=O and carbon; weak for adsorbates; fluorescence can swamp it.
HREELS: inelastic scattering of low-energy electrons from a flat surface in UHV. Sub-monolayer sensitivity down to very low wavenumber, and impact scattering sees modes that IRRAS cannot. Resolution is typically tens of cm⁻¹, much coarser than IR.